Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Melt Index Determination Load Test: Principles, Standards, and Procedures

Melt index determination load test measures the melt flow rate (MFR/MVR) of thermoplastic materials under a specified temperature and load, providing essential data for quality control, material grading, and process optimization. This article explains the testing principle, standard conditions, sample requirements, methods, and applications based on ISO 1133, ASTM D1238, and GB/T 3682 standards.

Technical Overview

The melt index determination load test, also known as the melt flow index (MFI) test or melt flow rate (MFR) test, is a fundamental rheological measurement used to characterize the flow behavior of thermoplastic polymers in the molten state. During the test, a polymer sample is heated to a specified temperature inside a cylindrical barrel and extruded through a standardized die by applying a dead load to a piston. The mass or volume of extrudate collected over a defined time interval is used to calculate the melt flow rate, expressed in grams per 10 minutes (g/10 min) for melt mass-flow rate (MFR) or cubic centimeters per 10 minutes (cm³/10 min) for melt volume-flow rate (MVR).

The test is performed using an extrusion plastometer (melt indexer) consisting of a heated barrel with an internal diameter of approximately 9.55 mm, a weighted piston, and a tungsten carbide or hardened steel die with a bore of 2.095 mm diameter and 8.0 mm length. The applied load is generated by calibrated weights mounted on the piston, and the standard test loads include 1.2 kg, 2.16 kg, 3.8 kg, 5 kg, 10 kg, and 21.6 kg. The combination of temperature and load is selected according to the material type and the relevant standard, and the resulting shear rate approximates the low-shear processing regime, making the melt index a practical indicator of processability in extrusion, injection molding, and other melt-processing operations.

The principal international and national standards governing this test include ISO 1133-1 and ISO 1133-2 (Plastics – Determination of the melt mass-flow rate MFR and melt volume-flow rate MVR of thermoplastics), ASTM D1238 (Standard Test Method for Melt Flow Rates of Thermoplastics by Extrusion Plastometer), GB/T 3682.1 and GB/T 3682.2, and JIS K 7210. Because the melt index is sensitive to molecular weight and molecular weight distribution, the test is widely used for incoming material inspection, grade identification, batch-to-batch consistency verification, and detection of polymer degradation.

Testing Samples

A wide range of thermoplastic materials can be evaluated by the melt index load test. Samples are typically supplied as pellets, granules, powders, or finely cut pieces taken from molded or extruded parts. The required sample mass for a single determination is generally 3 to 8 grams, and sufficient material should be provided to allow at least three replicate determinations. Hygroscopic materials must be dried before testing in accordance with the material specification or the relevant product standard.

Polyolefins

Polyethylene (PE), including LDPE, LLDPE, and HDPE, is commonly tested at 190°C with a 2.16 kg load. For high-density polyethylene with very low flow rates, a high-load condition of 190°C with a 21.6 kg load (high-load melt index, HLMI) is frequently applied. Polypropylene (PP), including homopolymer and impact copolymer grades, is typically tested at 230°C with a 2.16 kg or 5.0 kg load.

Styrenic Polymers

Polystyrene (PS) is usually evaluated at 200°C with a 5.0 kg load, while acrylonitrile butadiene styrene (ABS) and styrene-acrylonitrile (SAN) are commonly tested at 220°C with a 10 kg load. Filled or glass-reinforced styrenic compounds may require adjusted conditions agreed between the parties.

Engineering Thermoplastics

Polycarbonate (PC) is tested at 300°C with a 1.2 kg load. Polyoxymethylene (POM) is tested at 190°C with a 2.16 kg load. Polyamide (PA6) is typically tested at 235°C and PA66 at 275°C, and these materials must be thoroughly dried prior to testing to avoid hydrolytic degradation and bubble formation in the extrudate. Polyethylene terephthalate (PET) and polybutylene terephthalate (PBT) are tested at 250°C with a 2.16 kg load after careful drying.

Other Thermoplastics

Polymethyl methacrylate (PMMA), thermoplastic polyurethane (TPU), polyolefin elastomers (POE), ethylene-vinyl acetate copolymers (EVA), fluoropolymers such as FEP and PFA, and various thermoplastic compounds and masterbatches can also be tested using the condition specified in the material datasheet or product standard.

Testing Items

The melt index determination load test covers the following measurable parameters:

  • Melt mass-flow rate (MFR), expressed in g/10 min, determined by weighing the extrudate collected over a timed interval.
  • Melt volume-flow rate (MVR), expressed in cm³/10 min, determined by measuring the piston travel distance over a timed interval.
  • Flow rate ratio (FRR), calculated as the ratio of MFR or MVR values obtained at two different loads at the same temperature, providing an indication of molecular weight distribution and shear sensitivity.
  • Melt density at the test temperature, derived from paired MFR and MVR measurements.
  • High-load melt index (HLMI) for materials with extremely low flow rates, typically performed at 190°C with a 21.6 kg load.

Testing Methods

The test is performed in accordance with ISO 1133-1/1133-2, ASTM D1238, GB/T 3682.1/3682.2, or JIS K 7210. The equipment is calibrated for temperature, load, and dimensional accuracy, and the barrel and piston are cleaned between determinations to eliminate residue that could affect results.

Method A – Mass Measurement Procedure

In Method A, a pre-weighed quantity of sample is loaded into the preheated barrel and compacted with the piston to remove entrapped air. After a specified preheat period of approximately 5 to 7 minutes (depending on the standard and material), the selected load is applied to the piston. Once the lower reference mark on the piston reaches the top of the barrel, the extrudate is cut off and discarded. Successive extrudate segments are then cut at timed intervals (for example, 15, 30, or 60 seconds depending on the flow rate), collected, cooled, and weighed on an analytical balance. The melt mass-flow rate is calculated as MFR (g/10 min) = 600 × m / t, where m is the average mass of the extrudate in grams and t is the cut interval in seconds.

Method B – Piston Displacement Procedure

In Method B, an automatic displacement transducer or optical encoder measures the distance traveled by the piston over a defined time period. The melt volume-flow rate is calculated directly from the piston travel, the barrel cross-sectional area, and the time interval. If the melt density at the test temperature is known or simultaneously determined, MVR can be converted to MFR using the relationship MFR = MVR × melt density. Method B avoids manual cutting and weighing, reduces operator influence, and is well suited to materials with high flow rates and to automated instruments.

Sample Preparation and Conditioning

  • Materials must be free from moisture, contamination, and volatile components that could generate bubbles in the extrudate.
  • Hygroscopic polymers such as PA, PC, PET, PBT, and ABS must be dried prior to testing according to the material specification.
  • The sample should be preconditioned at the test temperature for the time specified in the standard to ensure complete melting and thermal equilibrium.
  • A minimum of three valid determinations is typically performed, and the individual values must agree within the reproducibility limits stated in the standard.
  • Extrudate segments containing visible bubbles must be discarded and the measurement repeated.

Typical Standard Test Conditions

  • PE: 190°C / 2.16 kg (general grades); 190°C / 21.6 kg (high-load condition).
  • PP: 230°C / 2.16 kg; 230°C / 5.0 kg for certain grades.
  • PS: 200°C / 5.0 kg.
  • ABS: 220°C / 10 kg.
  • PC: 300°C / 1.2 kg.
  • POM: 190°C / 2.16 kg.
  • PET: 250°C / 2.16 kg.
  • PMMA: 230°C / 3.8 kg.

Applications

Melt index data obtained from load testing support numerous technical and commercial activities across the plastics industry:

  • Incoming material inspection and verification that supplied resin lots conform to datasheet flow specifications.
  • Quality control during polymerization and compounding, where melt index is used to confirm reaction consistency and additive dispersion.
  • Material grade identification and differentiation, since flow rate correlates directly with molecular weight for a given polymer family.
  • Detection of thermal or oxidative degradation in recycled materials, reprocessed regrind, and aged polymers, indicated by elevated melt flow values.
  • Process optimization for extrusion, film blowing, injection molding, blow molding, fiber spinning, and wire coating.
  • Tooling and process design support, where flow rate ratios guide the selection of processing windows and shear-sensitive applications.
  • Product certification, supplier qualification, and failure analysis investigations conducted by accredited third-party laboratories.
  • Research and development of new resin grades, modifiers, and masterbatch formulations, where flow behavior is a primary screening criterion.

FAQ

What is the difference between MFR and MVR? MFR is the mass of extrudate expressed in g/10 min and requires weighing the collected extrudate, while MVR is the volume of extrudate expressed in cm³/10 min and is determined from piston displacement. The two values are related through the melt density at the test temperature.

Why are different loads used for different materials? The load is selected so that the measured flow rate falls within the sensitivity range of the method. Low-molecular-weight, easy-flowing polymers are measured with lighter loads, while stiff, high-molecular-weight materials require heavier loads to produce a measurable extrudate within a practical time.

How much sample is required for a test? Typically 3 to 8 grams are needed for a single determination, and a minimum total of about 20 to 25 grams is recommended to allow replicate measurements and retests.

Do all materials need drying before testing? No. Polyolefins such as PE and PP are generally not hygroscopic and usually do not require drying, whereas PA, PC, PET, PBT, and ABS must be dried to prevent bubble formation, hydrolytic degradation, and inaccurate results.

What do higher or lower melt index values indicate? A higher melt index indicates lower melt viscosity and generally lower molecular weight, corresponding to easier flow. A lower melt index indicates higher molecular weight, greater melt strength, and improved mechanical performance in many applications.

How long does the test take? A single determination typically takes 20 to 40 minutes, including preheating, loading, and measurement. A complete test report with replicate determinations is usually completed within one working day by accredited third-party laboratories.

Why Choose ZKGX?

  • State-of-the-art analytical equipment