Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

NBR (Nitrile Rubber) Compression Set Testing: Methods, Standards and Technical Guide

Nitrile rubber (NBR) compression set testing evaluates the ability of nitrile butadiene rubber components to recover their original thickness after prolonged compressive strain, which is one of the most critical indicators of long-term sealing reliability. Conducted in accordance with ISO 815-1, ASTM D395 and GB/T 7759.1, this test is widely used to qualify O-rings, gaskets and hydraulic seals for automotive, oil and gas, and general industrial applications. This technical guide explains the sample requirements, test procedures, calculation formulas, typical test conditions and acceptance criteria for NBR compression set evaluation.

Technical Overview

Compression set is defined as the residual deformation remaining in an elastomer after it has been compressed under a specified deflection or load for a defined period of time and then allowed to recover. For nitrile butadiene rubber (NBR, also known as nitrile rubber or Buna-N), compression set testing is one of the most important performance evaluations because NBR is predominantly used in sealing applications where sustained contact pressure is essential for leak prevention.

When an NBR seal is installed in a groove and compressed between mating surfaces, it relies on its elastic recovery force to maintain a seal. Over time, physical stress relaxation and chemical degradation of the polymer network cause the material to lose part of its original thickness. If the compression set becomes excessive, contact pressure drops below the level required for sealing, resulting in leakage. A lower compression set value therefore indicates better long-term sealing capability.

  • Compression set is expressed as a percentage; lower values indicate better elastic recovery
  • Test results are strongly influenced by temperature, test duration, crosslink density and cure system
  • Peroxide-cured NBR compounds generally exhibit lower compression set than sulfur-cured compounds
  • Testing can be performed at ambient, elevated or low temperatures depending on the service environment

Testing Samples

Standard Molded Cylindrical Buttons

The preferred specimen for compression set testing is a solid cylindrical button molded directly from the compound under evaluation. In accordance with ISO 815-1 and GB/T 7759.1, Type A specimens measure 29.0 mm in diameter and 12.5 mm in height, while Type B specimens measure 13.0 mm in diameter and 6.3 mm in height. Specimens must be flat, parallel and free from voids, blisters, porosity and surface defects that could bias thickness measurements.

O-Ring Specimens

Finished O-rings may be tested directly when the objective is to evaluate the actual manufactured product rather than a laboratory compound. O-ring compression set testing is typically conducted with a 25% reduction in cross-section diameter using appropriate fixtures, following practices consistent with ASTM D1414. Testing actual O-rings captures the combined influence of the compound, molding process and post-cure conditions.

Finished Components and Custom Specimens

Gaskets, washer profiles, seals and other finished parts can be evaluated in application-representative fixtures. For custom specimens, a minimum thickness of approximately 6 mm is recommended so that thickness changes can be measured with adequate resolution using instruments accurate to 0.01 mm. Specimens should be tested in the orientation in which they will be compressed in service.

Testing Items

Compression set evaluation for NBR materials typically covers the following test items, selected according to the intended service conditions:

  • Compression set under constant deflection at elevated temperature (most common method for NBR)
  • Compression set under constant force (dead-load method)
  • Low-temperature compression set and recovery behavior
  • Compression set after prolonged aging, such as 168 hours or 1000 hours of exposure
  • Compression set after fluid immersion, such as testing specimens following oil or fuel resistance exposure
  • Comparative evaluation of sulfur-cured versus peroxide-cured NBR compounds
  • Verification of post-cure effectiveness and batch-to-batch production consistency

The principal reported result is the compression set percentage calculated from the original thickness, the recovered thickness and, for constant-deflection testing, the compressed height defined by the fixture spacers.

Testing Methods

Applicable Standards

  • ISO 815-1: Rubber, vulcanized or thermoplastic — Determination of compression set — Part 1: At ambient or elevated temperatures
  • ISO 815-2: Determination of compression set — Part 2: At low temperatures
  • ASTM D395: Standard Test Methods for Rubber Property — Compression Set (Method A: constant force; Method B: constant deflection)
  • ASTM D1414: Standard Test Methods for Rubber O-Rings, including compression set of O-ring specimens
  • GB/T 7759.1 and GB/T 7759.2: Chinese national standards technically aligned with ISO 815-1 and ISO 815-2
  • JIS K 6262: Japanese industrial standard covering compression set of rubber materials

Specimen Conditioning

Specimens should be allowed to rest after vulcanization for a minimum of 16 hours, and preferably 72 hours, before testing. The interval between molding and testing should not exceed four weeks for laboratory-molded sheets. Prior to measurement, specimens are conditioned in a standard laboratory atmosphere of 23 ± 2 °C and 50 ± 5% relative humidity for at least 3 hours. The original thickness is measured at a minimum of three points and averaged.

Test Procedure (Constant Deflection, Method B)

The constant-deflection method is the standard approach for NBR compression set evaluation:

  • Measure and record the original specimen thickness t0
  • Place the specimen between rigid, parallel steel plates fitted with spacers sized to produce the target compression, typically 25% of the original thickness
  • Assemble the fixture and tighten to a defined torque so the plates rest firmly on the spacers
  • Place the assembled fixture in a circulating-air oven maintained at the selected test temperature for the specified duration
  • At the end of exposure, remove the fixture, release the specimen immediately and allow it to recover at standard laboratory temperature for 30 ± 1 minutes
  • Measure the recovered thickness t1 at the same locations used for the original measurement
  • Test a minimum of three specimens and report the median value together with individual results

Calculation of Results

For compression set under constant deflection (Method B), the compression set CB is calculated as CB = (t0 − t1) / (t0 − ts) × 100%, where t0 is the original thickness, t1 is the recovered thickness after the recovery period, and ts is the thickness defined by the fixture spacers. For compression set under constant force (Method A), the result is calculated as CA = (t0 − t1) / t0 × 100%. A result of 0% represents complete recovery, while 100% indicates total loss of recovery capability.

Typical Test Conditions for NBR

Because standard NBR is generally suitable for continuous service up to approximately 100 °C with intermittent exposure up to about 120 °C, common test conditions include the following:

  • 70 °C or 100 °C for 22–24 hours: routine quality control screening
  • 100 °C for 70 hours: widely used acceptance condition for NBR seals and O-rings
  • 120 °C for 70 hours: evaluation of heat-resistant or peroxide-cured NBR compounds
  • 168 hours or 1000 hours at 70–100 °C: long-term aging and lifetime assessment
  • Low-temperature recovery testing at −10 °C to −40 °C according to ISO 815-2, with recovery measured at the test temperature

Typical Result Ranges

Conventional sulfur-cured NBR compounds commonly show compression set values in the range of approximately 15% to 30% after 70 hours at 100 °C, while well-formulated peroxide-cured compounds with optimized crosslink density can achieve values below 15% under the same conditions. Acceptance limits are defined by the product specification, the applicable material line-callout in standards such as those based on ASTM D2000 classification, or by agreement between supplier and purchaser.

Applications

Compression set data for NBR directly support design, qualification and quality decisions across industries in which nitrile rubber is the material of choice for oil and fuel resistance:

  • Automotive engineering: valve cover gaskets, crankshaft seals, fuel system seals, O-rings and diaphragms exposed to sustained compression and engine-bay heat
  • Hydraulic and pneumatic systems: rod seals, piston seals, backup rings and couplings where pressure retention depends on long-term contact force
  • Oil and gas equipment: seals, packer elements and downhole components requiring resistance to hydrocarbons and elevated temperature
  • General industrial machinery: flange gaskets, pipe seals, pump seals and damping elements under permanent bolt load
  • Material development: comparison of compound formulations, cure systems, filler loadings and post-cure treatments
  • Production quality control: batch release testing and verification of molding process consistency in accredited third-party laboratories or in-house facilities

FAQ

What is a good compression set value for NBR?

For NBR tested for 70 hours at 100 °C with 25% deflection, values below approximately 20% are generally considered acceptable for demanding sealing duties, while values below 15% indicate excellent recovery, typically achieved with peroxide-cured or efficiently sulfur-cured compounds. The applicable specification should always be consulted, since acceptance limits vary by application and material class.

What is the difference between ASTM D395 Method A and Method B?

Method A applies a constant force to the specimen using a dead-weight or spring apparatus, while Method B compresses the specimen to a constant deflection, typically 25%, maintained by a bolted fixture with spacers. Method B is the more widely used procedure for seal materials because it directly simulates the fixed squeeze of an installed O-ring or gasket.

Why is a 25% compression level commonly used?

A 25% deflection approximates the typical squeeze applied to O-rings and seals in real installations and produces measurable, reproducible deformation without mechanically damaging the specimen. Standards such as ISO 815-1 and ASTM D395 define this level as the reference condition unless a product specification requires otherwise.

How can the compression set performance of NBR be improved?

Effective measures include switching from conventional sulfur curing to peroxide or efficient vulcanization systems, optimizing crosslink density, reducing extractable plasticizer content, selecting appropriate carbon black grades and loadings, applying a post-cure to complete crosslinking, and avoiding unnecessary service temperatures above the material rating.

Can compression set testing be combined with fluid resistance testing?

Yes. A common practice is to immerse NBR specimens in reference oils, fuels or service fluids at elevated temperature, following oil-resistance procedures, and then perform compression set evaluation either after immersion or on separately exposed specimens. This combination reveals how fluid-induced swelling and extraction affect the sealing recovery of the compound under realistic conditions.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing