Ubicación: Global + English
Global Global Algérie Français Algeria English Angola Português Angola English Argentina Español Argentina English Australia English Austria Deutsch Austria English Azerbaijan English Azerbaijan Русский Bahrain English Bangladesh English Belgium English Belgium Français Belgium Nederlands Brazil Português Brazil English Bulgaria български Bulgaria English Cameroon English Cameroon Français Canada English Canada Français Chile Español Chile English China 中文 China 日本語 China English Colombia Español Colombia English Croatia English Czech Republic Čeština Czech Republic English Denmark English Djibouti English Ecuador Español Ecuador English Egypt English Estonia English Ethiopia English Finland Suomi Finland English France Français France English Georgia English Georgia Русский Germany Deutsch Germany English Ghana English Greece Ελληνικά Greece English Guatemala Español Guatemala English Hong Kong, China English Hong Kong, China 中文 Hungary Magyar Hungary English India English Indonesia English Iraq English Ireland English Italy Italiano Italy English Ivory Coast Français Ivory Coast English Japan 日本語 Japan English Jordan English Kazakhstan Русский Kazakhstan English Kenya English Kuwait English Kyrgyzstan Русский Kyrgyzstan English Latvia English Lithuania English Malaysia English Mauritius English Mauritius français (Maurice) Mexico Español Mexico English Moldova Română Moldova English Mongolia English Morocco English Morocco Français Mozambique Português Mozambique English Netherlands Nederlands Netherlands English New Zealand English Nigeria English Norway English Oman English Pakistan English Paraguay Español Paraguay English Peru Español Peru English Philippines English Poland Polski Poland English Portugal Português Portugal English Qatar English Republic of Korea 한국어 Republic of Korea English Romania Română Romania English Saudi Arabia English Serbia Српски Serbia English Singapore English Slovakia English Slovenia English South Africa English Spain English Spain Español Sri Lanka English Sweden English Switzerland Deutsch Switzerland Français Switzerland Italiano Switzerland English Tanzania English Thailand ไทย Thailand English Togo English Togo Français Tunisia English Tunisia Français Türkiye Türkçe Türkiye English Turkmenistan Русский Turkmenistan English Ukraine Українська Ukraine English United Arab Emirates English United Kingdom English Uruguay Español Uruguay English USA English Uzbekistan English Uzbekistan Русский Vietnam Tiếng Việt Vietnam English

Determination of Linear Expansion of Concrete: Standards, Methods, and Applications

Determination of linear expansion in concrete is an essential laboratory procedure that quantifies how concrete specimens change in length under drying, autogenous, and thermal conditions. Testing in accordance with recognized standards such as ASTM C157, EN 12390-16, and GB/T 50082 enables engineers to assess cracking risk, design movement joints, and verify the long-term dimensional stability of concrete structures. This article explains the technical principle, sample requirements, testing items, measurement methods, and practical applications of concrete linear expansion determination.

Technical Overview

Linear expansion determination measures the one-dimensional length change of hardened concrete specimens exposed to controlled environmental conditions. The measured change may be an expansion or a contraction (shrinkage), and the result is typically expressed as a percentage of the original gauge length or as microstrain. Understanding this behavior is fundamental to concrete durability engineering, because restrained length change is one of the primary causes of cracking in concrete structures.

Two distinct mechanisms are evaluated under the general term of linear length change. The first is moisture-driven deformation, which includes drying shrinkage, autogenous shrinkage, and swelling during water storage. The second is temperature-driven deformation, characterized by the linear coefficient of thermal expansion (CTE), which describes how much the concrete elongates or shortens per unit length per degree of temperature change. Typical ordinary concrete exhibits a CTE in the range of approximately 8 to 12 × 10⁻⁶ per degree Celsius, while drying shrinkage strains commonly fall between 200 and 800 microstrain depending on mix proportions, aggregate type, and curing history.

Established test methods for this determination are published by leading standards organizations, and accredited third-party laboratories routinely perform these tests for specification compliance and research purposes. The most widely referenced standards include:

  • ASTM C157 – Standard Test Method for Length Change of Hardened Hydraulic-Cement Mortar and Concrete
  • ASTM C426 – Standard Test Method for Linear Drying Shrinkage of Concrete Masonry Units
  • ASTM E228 – Standard Test Method for Linear Thermal Expansion of Solid Materials by Push-Rod Dilatometry
  • ASTM E831 – Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis
  • EN 12390-16 – Testing Hardened Concrete: Determination of the Shrinkage of Concrete
  • GB/T 50082 – Standard for Test Methods of Long-Term Performance and Durability of Ordinary Concrete
  • JIS A 1129 – Methods of Measurement for Length Change of Mortar and Concrete
  • ISO 1920 series – Testing of Concrete, including determination of drying shrinkage

Testing Samples

Cast Concrete Prisms

The most common specimen is a molded concrete prism fitted with stainless steel gauge studs at both ends. Square cross-sections of 100 mm by 100 mm with a length of approximately 500 mm are typical for tests following GB/T 50082, while ASTM C157 prescribes prisms with cross-sections of 75 mm, 100 mm, or 150 mm square and a nominal length of 285 mm between gauge points. Prisms are cast in steel molds, compacted by vibration or rodding, and covered to prevent moisture loss during initial curing.

Mortar and Paste Specimens

For binder characterization and mix design studies, smaller mortar prisms of 25 mm by 25 mm by 285 mm are used in accordance with ASTM C157 and ASTM C596. Cement paste and mortar specimens cast in corrugated plastic tubes may also be employed for very early-age autogenous strain measurement, following the principle of ASTM C1698.

Hardened Cores and Cylinders

Drilled cores or cast cylinders can be tested for the coefficient of thermal expansion by attaching gauge points or by placing the specimen in a dilatometer or a temperature-controlled water bath with an external displacement transducer. Core testing is particularly valuable when the thermal behavior of existing structures must be evaluated.

Concrete Masonry Units

Complete concrete blocks or sawn sections of units are measured for drying shrinkage in accordance with ASTM C426, which specifies conditioning from a saturated state to equilibrium at standard laboratory conditions.

Sealed Specimens

For autogenous shrinkage determination, specimens are sealed with wax, adhesive foil, or impermeable membranes immediately after casting to isolate deformation caused by self-desiccation from ordinary drying effects.

Testing Items

Linear expansion determination encompasses several specific measurable parameters, each corresponding to a distinct service condition or degradation mechanism:

  • Drying shrinkage strain – length reduction measured at defined ages while specimens are stored at controlled temperature and relative humidity
  • Autogenous shrinkage strain – self-desiccation deformation of sealed concrete, critical for high-performance and low water-cement ratio mixes
  • Immersion or wet-curing expansion – swelling measured while specimens are stored in water
  • Linear coefficient of thermal expansion (CTE) – expressed in 10⁻⁶ per degree Celsius or micrometers per meter per degree Celsius
  • Irreversible shrinkage and rewetting recovery – residual deformation after re-saturation of previously dried specimens
  • Length change of concrete masonry units – total drying shrinkage from saturated to equilibrium moisture condition
  • Residual carbonation-related length change – evaluated in specialized durability studies

Testing Methods

Specimen Preparation and Conditioning

Gauge studs are cast into the fresh concrete or attached afterward with rapid-setting adhesive. After demolding, specimens are cured in water or a moist room, typically to an age of 24 hours or as specified by the governing standard. A zero-length reading is taken using a calibrated reference or datum bar before the specimens are placed in the test environment. Standard conditioning atmospheres include 23 ± 2 °C with 50 ± 4 percent relative humidity per ASTM C157, and 20 ± 2 °C with 60 ± 5 percent relative humidity per EN 12390-16 and GB/T 50082.

Comparator Method

The classic measurement device is a length comparator consisting of a rigid frame, an anvil, and a dial gauge or digital linear variable differential transformer (LVDT) with a resolution of at least 0.002 mm. The specimen is seated on the anvil with one gauge stud in contact, and the reading is recorded. Measurements are repeated at specified ages, commonly 1, 3, 7, 14, 28, 56, and 90 days, and may continue to 180 days or one year for long-term evaluation. Each reading session begins and ends with a check against the reference bar to correct for instrument drift and thermal effects.

Dilatometry and Thermomechanical Analysis

For the coefficient of thermal expansion, a push-rod dilatometer in accordance with ASTM E228 or a thermomechanical analyzer in accordance with ASTM E831 applies a controlled heating or cooling cycle while continuously recording specimen length. The test is frequently performed over a range such as 10 °C to 60 °C, which represents typical environmental exposure of concrete structures, and at least two thermal cycles are run to confirm repeatability, with the first cycle sometimes discarded to eliminate initial moisture effects.

Water-Bath Frame Method

An alternative CTE approach places a prism or cylinder in a supporting frame equipped with a precision LVDT, submerged in a circulating water bath. The bath temperature is stepped through set points, for example 10 °C, 21 °C, and 32 °C, holding each point until the specimen reaches thermal equilibrium, and the length change is recorded at each step. This method is well suited to saturated specimens of larger aggregate size.

Embedded and Contact Instrumentation

For field monitoring and large-scale laboratory members, vibrating wire strain gauges or embeddable length-change transducers may be cast directly into the concrete. These devices provide continuous strain histories that complement discrete comparator readings and support early-age crack risk analysis.

Data Reduction and Calculation

Length change at any age is computed as the difference between the current reading and the initial reading, corrected by the reference bar values, divided by the initial gauge length. The result is expressed as a percentage or as strain in microstrain. The coefficient of thermal expansion is calculated as the slope of the length change versus temperature curve, dividing the stable length change by the product of the initial length and the corresponding temperature interval. Reportable results generally include the individual values, the mean, the measurement uncertainty, curing history, ambient conditions, and specimen geometry.

Applications

Linear expansion data serve a wide range of engineering and quality assurance purposes across the construction industry:

  • Movement joint design in buildings, bridges, pavements, and industrial floors, where joint spacing must accommodate predicted thermal and moisture-induced movement
  • Mass concrete engineering, including dam and thick foundation construction, where thermal expansion data feed into temperature control and crack mitigation plans
  • Precast concrete production, for verifying dimensional stability of elements before erection and ensuring dimensional fit on site
  • Repair and overlay compatibility, confirming that repair mortars and grouts have shrinkage and thermal behavior matched to the substrate concrete
  • Durability assessment and service-life prediction, since restrained shrinkage is directly linked to cracking, permeability, and ingress of aggressive agents
  • Mix design optimization, evaluating the influence of supplementary cementitious materials, aggregates, admixtures, and water-cement ratio on volume stability
  • Specification compliance and certification testing performed by accredited third-party laboratories for owners, contractors, and materials suppliers

FAQ

What is the linear expansion coefficient of normal concrete?

Most structural concretes made with siliceous river aggregates exhibit a coefficient of thermal expansion between 8 and 12 × 10⁻⁶ per degree Celsius. Mixtures containing limestone or lightweight aggregates tend toward the lower end of this range, while those with quartz-rich aggregates approach the higher end. The value should always be confirmed by testing for projects where movement control is critical.

What specimen sizes are commonly used?

Concrete prisms of 100 mm by 100 mm by 515 mm with embedded gauge studs are standard under GB/T 50082, prisms of 285 mm gauge length with 75 mm to 150 mm square sections are used per ASTM C157, and mortar prisms of 25 mm by 25 mm by 285 mm are used for binder evaluation. Cores and cylinders of 75 mm to 150 mm diameter are accepted for thermal expansion testing.

How long does the test take?

Drying shrinkage measurement is usually performed to at least 28 days of drying and frequently extended to 90 or 180 days because shrinkage develops gradually. Thermal expansion testing of a saturated specimen is typically completed within one to three days, including conditioning and multiple thermal cycles.

How do drying shrinkage and thermal expansion testing differ?

Drying shrinkage testing holds temperature and relative humidity constant and measures length change driven by moisture loss over time. Thermal expansion testing holds moisture condition constant and varies temperature, measuring the instantaneous elastic response. Both parameters are needed for a complete deformation analysis of concrete structures.

Why must a reference bar be used with a comparator?

The reference bar compensates for zero drift of the dial gauge or LVDT and for thermal expansion of the comparator frame itself. Taking readings on the reference bar immediately before and after each specimen measurement, at the same temperature, ensures that reported length changes reflect only the behavior of the concrete.

What acceptance limits are typical?

Acceptance criteria depend on the specification and application. Many structural specifications limit drying shrinkage at 28 days to values on the order of 400 to 600 microstrain, and repair products are often required to stay below specific limits at both early and later ages. The governing project documents should always be consulted for the applicable thresholds.

Why Choose ZKGX?

  • State-of-the-art analytical equipment
  • Highly qualified scientific team
  • Fast turnaround time
  • Competitive pricing